MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M Diamond Grade™ 983 Conspicuity Markings
Categories: Polymer; Adhesive

Material Notes: 3M™ Diamond Grade™ Conspicuity Markings Series 983 are highly retrorflective micro-prismatic markings designed to mark the sides and rear of vehicles for enhanced visibility and detection. The reflective marking consists of prismatic lenses that are formed in a transparent synthetic resin, sealed and cracked with a pressure-sensitive adhesive clear poly liner. Applied to properly prepared surfaces Diamond Grade markings should provide seven years of field performance.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brightness 5.00 %5.00 %5 Red; ASTM E1164
 45.0 %45.0 %Whiteness Reflective Limit Y
Thickness 356 - 457 microns14.0 - 18.0 milCaliper
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.438 kN/m2.50 pli12 in/min, 90° pullback, FRP
 0.526 kN/m3.00 pli12 in/min, 90° pullback, Prepainted panel
 0.526 kN/m3.00 pli12 in/min, 90° pullback, Tedlar™
 0.614 kN/m3.50 pli12 in/min, 90° pullback, Aluminum Rail
 0.929 kN/m5.30 pli12 in/min, 90° pullback, Degreased aluminum
 1.05 kN/m6.00 pli12 in/min, 90° pullback, Stainless steel
 
Optical PropertiesMetricEnglishComments
Gloss 100 %100 %85°; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM34789 / 169536

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.