MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ChevronTexaco Polystar® Synthetic 4602 NLGI Grade
Categories: Fluid; Lubricant; Urea Gellant

Material Notes: Texaco Polystar Synthetic 4602 delivers value through:
  • Wide application range — Suitable for high rpm operation, operating temperatures ranging from -40°C to 230°C (-40°F to 446°F) and offers excellent rust protection in the presence of both salt and fresh water.
  • Excellent oxidation stability — Provides exceptional bearing life at high operating temperatures.
  • Excellent rust and corrosion protection — Provides superior rust protection as defined by ASTM D 1743.

Texaco Polystar Synthetic 4602 is a high temperature, synthetic based ball and roller bearing grease.

Texaco Polystar Synthetic 4602 passes the ASTM D 1743 73 rust test with 5% synthetic seawater. It provides longer bearing life under high speed and high temperature operation than most other widely used antifriction bearing greases. ASTM D 3527 wheel bearing life testing shows that the B50 life of a bearing lubricated with Texaco Polystar Synthetic 4602, operating at 160°C (320°F), is 300 - 460 hours, an outstanding result. FAG FE-9 ball bearing testing demonstrates that the Texcaco Polystar Synthetic 4602 will provide continuous duty lubrication at temperatures up to 180°C (356°F) with short exposure capability up to 230°C (446°F).

Texaco Polystar Synthetic 4602 is recommended in high temperature applications where other greases harden and will not perform, including:

  • A wide range of automotive and industrial applications.
  • Use in antifriction bearings operating at high speeds (10,000 rpm and greater).
  • Where the operating temperatures are on the order of 160°C (320°F) and higher.
  • Where there is a likelihood that water or salt water will get into the bearings.

It performs satisfactorily in bearings at temperatures as low as -40°C (-40°F).

Other applications where Texaco Polystar Synthetic 4602 is recommended include:

  • Bearings on air-conditioning units in homes and other buildings.
  • Unsealed electric motor bearings operating under moist conditions as well as bearings in generators, alternators and fans.
  • Bearings found in the dryer section of paper machine operations.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
  2. Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
  3. Determined on mineral oil extracted by vacuum filtration.

CPS Number: 222016; MSDS Number: 8999

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 140Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 2413 SUSSee Note 3.
Saybolt Viscosity at 210°F 201 SUSSee Note 3.
Kinematic Viscosity at 40°C (104°F) 460 cStSee Note 3.
Kinematic Viscosity at 100°C (212°F) 41.5 cStSee Note 3.
 
Mechanical PropertiesOriginal ValueComments
Penetration P(60), 1/10 mm 280Unknown Amount of Work, 25°C (77°F)
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °CSee Note 2.
Minimum Service Temperature, Air -40.0 °CSee Note 1.
Dropping Point 243 °C
 
Descriptive Properties
ColorBeige
TextureSmooth, Buttery
Thickener, %15Polyurea

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Polystar® RB NLGI Grade 2
ChevronTexaco Polystar® CVJ
Celanese FORTRON 1120L4 PPS, 20% Specialty

WTEXA265 / 77144

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.