MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Belsil® OW 1500 Polydimethylsiloxane-Glycol Copolymer
Categories: Fluid; Polymer

Material Notes: BELSIL® OW 1500 is a copolymer of polydimethylsiloxane and organic glycol.

Application: In hair-fixative compositions, it acts as resin plasticizer, reducing brittleness and flaking of organic resins. In shampoos and shower gels, this silicone surfactant helps to stabilize the foam, confers mild conditioning benefits on hair and skin and promotes formation of clear products. In creams and lotions, it acts as co-emulsifiers providing oil-in-water emulsification benefits, improving skin feel and product stability.

INCI name: proposed: PEG/PPG-20/20 Copolymer, PEG/PPG-20/20 Dimethicone

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccDIN 51757
Kinematic Viscosity 800 cSt
 
Thermal PropertiesOriginal ValueComments
Flash Point 120 °CISO 2719
Ignition Temperature >= 400 °CDIN 51794
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.452
 
Descriptive Properties
Appearanceyellowish liquid
Cloud point38.5-40.5%1% solution in water
Solubility4-Methylbenzylidene camphor>10%
 BELSIL® DM 0.65insoluble
 BELSIL® DM 100insoluble
 BELSIL® PDM 20, 350 VP 1000insoluble
 Benzophenone-3>10%
 C12-15 alkyl benzoates>10%
 C9-13 isoparaffin1-10%
 Castor oil>10%
 Cocoglycendes>10%
 Cyclopentasiloxaneinsoluble
 Decyl oleate1-10%
 Ethanol>10%
 Ethyl acetate1-10%
 Ethylhexyl Methoxycinnamate>10%
 Ethylhexyl Salicylate>10%
 Glycerolinsoluble
 Isopropyl myristate>10%
 Lanolin oil1-10%
 Mineral oil (high-viscosity)1-10%
 Mineral oil (low-viscosity)1-10%
 Octyl dodecanol>10%
 Oleyl alcohol>10%
 Olive oilinsoluble
 Polyglyceryl-2 Sesquisostearate>10%
 Propylene glycolinsoluble
 Sorbitan Trioleate>10%
 Water>10%
 Wheat germ oilinsoluble

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ FLD 48 V 750 to 1000000 Polydimethylsiloxane Silicone Oils
Lubrizol LifeSciences Tecophilic® TG-500 Hydrophilic TPU Hydrogel
Elkem (Bluestar Silicones) BLUESIL™ FLD 48 V 135000 Polydimethylsiloxane Fluid
Elkem (Bluestar Silicones) BLUESIL™ FLD 48 V 100 Polydimethylsiloxane Fluid
BASF Ecoflex® C1200 F Blend Biodegradable Polyester

PWACK9033 / 204562

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.