MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Designer Molecules BMI-689 Liquid Bismaleimide
Categories: Fluid

Material Notes: Description: BMI-689 is a unique low viscosity liquid bismaleimide based on a non-hydrogenated dimer diamine backbone. It can be homo-cured via UV or free radical initiators to form tough, hydrophobic, cross-linked polyimides. The material has excellent low pH hydrolytic resistance and thermal stability. The amorphous nature of this BMI allows it to be used in a variety of applications including mixed cure systems (e.g. epoxy and BMI), mixed BMI systems or where a low viscosity, free radical cured resin is required. It is soluble in most aromatic and aliphatic solvents such as toluene, xylene, NMP, etc.

Highlights:

  • Low viscosity liquid BMI
  • High adhesion to various substrates
  • Hydrophobic
  • Superior thermal stability

Information provided by Designers Molecules

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 1000 - 2000 cP1000 - 2000 cPCone and Plate @ 5 rpm
Molecular Weight 689 g/mol689 g/mol
Storage Temperature <= 5.00 °C<= 41.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 0.500 GPa72.5 ksicured with 2% Dicumyl Peroxide
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.43
@Frequency 2.00e+10 Hz
2.43
@Frequency 2.00e+10 Hz
Cavity Perturbation Method
Dissipation Factor 0.0020
@Frequency 2.00e+10 Hz
0.0020
@Frequency 2.00e+10 Hz
Cavity Perturbation Method
 
Thermal PropertiesMetricEnglishComments
CTE, linear 200 µm/m-°C111 µin/in-°Fa2
Glass Transition Temp, Tg <= 0.000 °C<= 32.0 °F
Decomposition Temperature >= 400 °C>= 752 °Fneat, in air
 
Descriptive Properties
AppearanceYellow to amber liquid
Weight Loss<1.0%@ 300°C (neat, in air)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDESGN003 / 255367

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.