MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC FLEX NORYL™ Resin WCA901 Polyphenylene Ether + TPE (PPE+TPE) (Europe)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyphenylene Ether/PPO

Material Notes: FLEX NORYL™ WCA901 resin is a flexible, non-reinforced extrudable blend of Polyphenylene Ether (PPE) + Thermoplastic Elastomer (TPE). This material contains non-halogenated flame retardant and performance capable of meeting UL VW-1 requirements, 105C end use temperature rating, and heat deformation performance as defined by UL 1581. FLEX NORYL WCA901 resin is intended for evaluation in wire and cable applications. It has a Shore A Hardness reading of 91 and exhibits superior thermal stability, very low water absorption, good electric properties, and low specific gravity. Processing is typically conducted on standard extrusion equipment, and UL 1581 testing is conducted on 2.0mm wire with 0.12mm X 20 stranded copper conductor.

Features: Flexible,Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Thin Wall,Non-Halogenated,Non-Chlorinated,Non-Brominated,Good Processability,Ductile

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Moisture Absorption 0.0200 %0.0200 %Wire Coating Extrusion
Melt Flow 10 g/10 min
@Load 10.0 kg,
Temperature 250 °C
10 g/10 min
@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 919130s reading; ASTM D2240
Tensile Strength at Break 22.0 MPa3190 psi50 mm/min; ISO 527
 23.0 MPa3340 psi50 mm/min; ASTM D638
 26.0 MPa3770 psiUL 1581
 27.0 MPa3920 psiafter 7days @136°C; UL 1581
Elongation at Break 95 %95 %50 mm/min; ISO 527
 110 %110 %50 mm/min; ASTM D638
 127 %127 %after 7days @136°C; UL 1581
 190 %190 %UL 1581
Flexural Modulus 0.390 GPa56.6 ksi12.5 mm/min, 100 mm span; ASTM D790
 0.390 GPa56.6 ksi12.5 mm/min; ISO 178
Tear Strength 13.0 kN/m74.2 pliISO 6383
Heat Distortion 15 %
@Load 0.250 kg,
Temperature 121 °C
15 %
@Load 0.551 lb,
Temperature 250 °F
UL 1581
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.10e+15 ohm-cm5.10e+15 ohm-cmASTM D257
Surface Resistance 4.20e+16 ohm4.20e+16 ohmASTM D257
Dielectric Constant 2.7
@Frequency 1e+6 Hz
2.7
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.0040
@Frequency 1e+6 Hz
0.0040
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 105 °C221 °FUL temperature rating; UL 1581
Brittleness Temperature <= -40.0 °C<= -40.0 °FASTM D746
Oxygen Index 27 %27 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Processing Temperature 15.0 - 45.0 °C59.0 - 113 °FWater Bath Temperature
 240 - 270 °C464 - 518 °FNeck Temperature
Feed Temperature 200 - 240 °C392 - 464 °F
Middle Barrel Temperature 240 - 270 °C464 - 518 °F
Die Temperature 240 - 270 °C464 - 518 °FWire Coating Extrusion
Melt Temperature 240 - 270 °C464 - 518 °FWire Coating Extrusion
Head Temperature 240 - 270 °C464 - 518 °FCross-head Temperature
 240 - 270 °C464 - 518 °F
Wire Preheat Temperature 80.0 - 150 °C176 - 302 °F
Drying Temperature 75.0 - 85.0 °C167 - 185 °FWire Coating Extrusion
Dry Time 5.00 - 7.00 hour5.00 - 7.00 hourWire Coating Extrusion
 12.0 hour12.0 hourCumulative; Wire Coating Extrusion
Screw Speed 15 - 85 rpm15 - 85 rpm
 
Descriptive Properties
Cooling Water Air Gap100-200 mm
Extruder Length/Diameter Ratio (L/D)22:1 to 26:1
Screen Pack150-100
VW-1PassUL 1581

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82059 / 290006

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.