MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ConocoPhillips Hydroclear® 100 Gas Compressor Fluid
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Hydroclear Gas Compressor Fluid is designed to lubricate rotary screw and reciprocating compressors in natural gas service. Conoco's high-quality hydrocracked base oil, combined with specially tailored additives, provides the protection against rust, corrosion, oxidation, wear and foaming needed to produce long and trouble-free service. The interaction between natural gas and hydrocarbon-based oils can lead to an effect known as “gas dilution.” This effect reduces the effective viscosity of the lubricant and is normally taken into account by using ISO 100 and 150 viscosity grade products. Experience has shown that Hydroclear Gas Compressor Fluid provides excellent service and value in applications for which the compressor outlet pressure is less than 150 psig, the specific gravity of the gas stream is less than 1.0, and the gas outlet temperatures are well above the condensation point of the gas.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 100100Viscosity Index
Saybolt Viscosity at 100°F 516 SUS516 SUS
Saybolt Viscosity at 210°F 65 SUS65 SUS
Kinematic Viscosity at 40°C (104°F) 99 cSt99 cSt
Kinematic Viscosity at 100°C (212°F) 11.2 cSt11.2 cSt
 
Mechanical PropertiesMetricEnglishComments
Four Ball Wear 0.400 mm0.0157 in
 
Thermal PropertiesMetricEnglishComments
Pour Point -34.4 °C-30.0 °F
Flash Point 254 °C490 °F
 
Descriptive Properties
ASTM Rust A&BPass
Copper Corrosion1A
FZGPass 9 Load StagesASTM D5182
Oxidation Resistance4000 hrs.ASTM D-943

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON275 / 75312

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.