MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Palm Labs Adhesives TURBO FUSE SERIES 130 CLEAR FLEXIBLE (100 Viscosity) Rapid Bonding Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 150 CLEAR FLEXIBLE advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performance has been tested with a variety of materials, and is recommended for a multitude of applications. The fast curing qualities make it especially desirable in high speed industrial production. TURBO FUSE SERIES 150 CLEAR FLEXIBLE is ideal for use in applications that require an easily handled medium viscosity adhesive that require flexibile bondness. Because of the 500 viscosity, it works especially well in medium fitting applications such as broken ceramic repair, unfinished metal to metal bonding, metal to rubber, and rubber to rubber, such as "O" ring repair/manufacture. This product is a very good, easy to handle general purpose adhesive.

Part Numbers for this data: 04-150CF, 10-150CF, 15-150CF, 20-150CF, 25-150CF, 30-150CF, 35-150CF

Soluble in Acetone, MEK, Amide, Methylene Chloride

Information provided by Palm Laboratories Adhesives

Key Words: CAS No: 7085-85-0
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccLiquid State
Viscosity 450 - 550 cPLiquid State
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80 - 90Cured State
Tensile Strength 725 psiCured State
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.58e+14 ohm-cm
Dielectric Constant 2.44
@Frequency 1e+6 Hz
Cured State
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °FCured State
Softening Point 300 °FCured State
Minimum Service Temperature, Air -65.0 °FCured State
Flash Point 170 - 200 °FLiquid State
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %clear; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 MonthLiquid State
 
Descriptive Properties
AppearanceClear LiquidLiquid State
 Clear-HardCured State
Base compound (Resin)Ethyl CyanoacrylateLiquid State
Gap Fill0.007"Cured State
Material Set Up Time<15 secRubber to Rubber
 20-40 secPhenolic to Phenolic
 5-15 secAluminum to Aluminum
 7-15 secPolycarbonate to Polycarbonate
 7-25 secSteel to Steel

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPALML026 / 135180

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.