MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical SBR 1721 High Acrylonitrile Polymer  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: SBR 1721 is an oil extended cold polymerization SBR with 37.5 parts of highly aromatic oil and styrene-butadiene copolymer of 40% bound styrene. Raw materials for this product are carefully chosen for the best physical properties. The aromatic oil and high percentage of styrene result in a good miscibility and processing behavior during extrusion and calendaring.

Applications: SBR 1721 is recommended for tire applications, especially where improved wet grip properties are required, and other applications include molded and extruded mechanical goods with low resilience.

CAS No: 9003-55-8

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/cc
Volatiles 0.20 %
Mooney Viscosity 55
@Temperature 100 °C
ML 1+4
Ash 0.20 %
 
Chemical PropertiesOriginal ValueComments
Styrene Content 40 %Bound
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 23.5 MPa
@Treatment Temp. 145 °C,
Time 2100 sec
ASTM D412
Elongation at Break 580 %
@Treatment Temp. 145 °C,
Time 2100 sec
ASTM D412
300% Modulus 110 kg(f)/cm²
@Treatment Temp. 145 °C,
Time 2100 sec
ASTM D412
 
Descriptive Properties
ColorDark Brown Bale
ComponentsHAF68.75, ASTM D3185
 SBR 1721137.5, ASTM D3185
 Stearic Acid1, ASTM D3185
 Sulfur1.75, ASTM D3185
 TBBS1.38, ASTM D3185
 ZnO3, ASTM D3185
Oil Analysis27.3%
Organic Acid5%
Rheometer15.0 mint'90, 160°C, 1° Arc, ASTM D5289
 19.0 lb-inMH, 160°C, 1° Arc, ASTM D5289
 3.0 lb-inML, 160°C, 1° Arc, ASTM D5289
 4.5 mints1, 160°C, 1° Arc, ASTM D5289
 8.5 mint'50, 160°C, 1° Arc, ASTM D5289
Soap0.1%

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLAY747 / 148757

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.