MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Formosa Plastics Formolene® FC2304E LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Product Description: Formolene® FC2304E is a low density polyethylene offering good balance of optical properties and draw down characteristics. Formolene® FC2304E is formulated with slip and antiblock for use in applications offering excellent extrusion processing and good optical properties.

Availability: North America

Additive: Antiblock: 1200 ppm; Slip: 900 ppm

Features: Good Optical Properties; Low Density

Uses: Bags; Film

Processing Method: Extrusion; Profile Extrusion

Information provided by Formosa Plastic Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ASTM D1505
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 1200 ppm1200 ppm
Slip Level 900 ppm900 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 10.3 MPa
@Thickness 0.0305 mm
1500 psi
@Thickness 0.00120 in
Blown Film; ASTM D882
Film Tensile Strength at Yield, TD 9.65 MPa
@Thickness 0.0305 mm
1400 psi
@Thickness 0.00120 in
Blown Film; ASTM D882
Film Elongation at Break, MD 180 %
@Thickness 0.0305 mm
180 %
@Thickness 0.00120 in
Blown Film; ASTM D882
Film Elongation at Break, TD 490 %
@Thickness 0.0305 mm
490 %
@Thickness 0.00120 in
Blown Film; ASTM D882
1% Secant Modulus  172 MPa
@Thickness 0.0305 mm
25000 psi
@Thickness 0.00120 in
MD, Blown Film; ASTM D882
 207 MPa
@Thickness 0.0305 mm
30000 psi
@Thickness 0.00120 in
TD, Blown Film; ASTM D882
Elmendorf Tear Strength MD 290 g
@Thickness 0.0305 mm
290 g
@Thickness 0.00120 in
Blown Film; ASTM D1922
Elmendorf Tear Strength TD 110 g
@Thickness 0.0305 mm
110 g
@Thickness 0.00120 in
Blown Film; ASTM D1922
Dart Drop Test 70.0 g
@Thickness 0.0305 mm
0.154 lb
@Thickness 0.00120 in
Blown Film; ASTM D1709
Film Tensile Strength at Break, MD 22.8 MPa
@Thickness 0.0305 mm
3300 psi
@Thickness 0.00120 in
Blown Film; ASTM D882
Film Tensile Strength at Break, TD 15.2 MPa
@Thickness 0.0305 mm
2200 psi
@Thickness 0.00120 in
Blown Film; ASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 5.2 %
@Thickness 0.0300 mm
5.2 %
@Thickness 0.00118 in
Blown Film; ASTM D1003
Gloss 71 %
@Thickness 0.0300 mm
71 %
@Thickness 0.00118 in
45°, Blown Film; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFPCR749 / 311442

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.