MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ITW Devcon® ALUMINIUM WEAR COMPOUND Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Aluminum-filled epoxy putty, for use where long lasting, non rusting, robust repairs to metal surfaces are required. Use on applications requiring an aluminum, non-rusting finish • Repairing aluminum castings, molds, parts and equipment.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 g/cc1.80 g/cc
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888
Compressive Strength 67.8 MPa9830 psi
Adhesive Bond Strength 17.8 MPa2580 psiAdhesive tensile shear strength
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 15.7 kV/mm399 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 50.0 °C122 °FTemperature Resistance - Wet
 120 °C248 °FTemperature Resistance - Dry
Shrinkage 0.50 %0.50 %Linear During cure
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min
@Temperature 65.0 °C
2.00 hour
@Temperature 149 °F
16 hrs @ 25°C plus 2 hours @ 65°C
Pot Life 50.0 min50.0 min
 
Descriptive Properties
Chemical/Solvent ResistanceAmmonia: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Cutting Oil: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Gasoline (Unleaded): poor30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Isopropyl Alcohol: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Methyl Chloride: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Methyl Ethyl Ketone: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hypochlorite 5% (bleach): very good30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric Acid 10%: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Xylene: fair30 day immersion at 75°F. Sample cured 7 days at RT
ColorDark Gray
Coverage1112cm²/Kg@ 5mm
Mix Ratio by volume4 to 1
Mix Ratio by weight9 to 1
Recoat Time4 hours
Specific Volume (in.³/lb)15.4
Viscosityputty

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWD9191 / 239701

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.