MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Wolf Kunststoff INKUPAL N100 B5A (dry)
Categories: Polymer; Thermoplastic

Material Notes:

Information provided by Wolf Kunststoff

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183
Water Absorption 3.0 %50%RF; DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82DIN 53505
Ball Indentation Hardness 170 MPaH358/30; DIN 2039
Tensile Strength at Break >= 50.0 MPaDIN EN ISO 527
Tensile Strength, Yield 80.0 MPaDIN EN ISO 527
Tensile Modulus 3200 MPaDIN EN ISO 527
Charpy Impact Unnotched >= 3.00 kJ/m²EN ISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.9
@Frequency 50 Hz
IEC 250
Dielectric Strength 20.0 kV/mmIEC 243
Dissipation Factor 0.020
@Frequency 50 Hz
IEC 112
Comparative Tracking Index 600 VIEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
@Temperature 20.0 - 60.0 °C
ISO E 830
Specific Heat Capacity 1.70 J/g-°C
Thermal Conductivity 0.230 W/m-KDIN 52612
Melting Point 220 °C
Maximum Service Temperature, Air 85.0 °Clong term; UL 746B
 160 °C3 h
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CDIN EN ISO 75
Flammability, UL94 HB
@Thickness 3.20 mm
 
Descriptive Properties
Machined partsApplicable
Rods up to øe (de)Applicable
Sheets up to max. thicknessApplicable
Tubes (hollow rods) up to øe (de)Applicable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZEDEX3017 / 250074

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.