MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Wacker Elastosil® LR 6255 F Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Solvent free, free flowing silicone rubber for coating, addition crosslinking.

Special features:

  • universal coating material
  • easy processing
Application: Manufacture of conveyor belts, electrical sleevings, protective clothing, bellow expansion joints, awnings, sunblinds, sports performance fabrics and medical fabrics.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³
Viscosity 70000 - 110000 cP70000 - 110000 cPdynamic
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3838DIN 53505
Tensile Strength at Break 5.00 MPa725 psiDIN 53504 S1/ISO 37
Elongation at Break 400 %400 %DIN 53504 S1/ISO 37
Tear Strength 7.80 kN/m44.5 pliASTM 624 B
Compression Set 70 %70 %DIN 53517
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.70e+14 ohm-cm3.70e+14 ohm-cmDIN VDE 0303
Dielectric Constant 3.2
@Frequency 60 Hz
3.2
@Frequency 60 Hz
DIN VDE 0303
Dielectric Strength 27.0 kV/mm686 kV/inDIN VDE 0303
Dissipation Factor 0.00014
@Frequency 60 Hz
0.00014
@Frequency 60 Hz
DIN VDE 0303
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %"Transparent" but manufacturer does not quantify.
 
Processing PropertiesMetricEnglishComments
Cure Time 3.00 min
@Treatment Temp. 150 °C
0.0500 hour
@Treatment Temp. 302 °F
Pot Life 10080 min10080 min
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 26 %26 %ASTM D2863-70
 
Descriptive Properties
Appearancetransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9169 / 204698

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.