MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elkem (Bluestar Silicones) SILCOLAPSE® 426R Silicone Emulsion
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: SILCOLAPSE® 426R is a water soluble 30% active defoamer designed for use in a variety of industrial applications. It effectively controls foam at concentrations as low as 10 ppm, even at elevated temperatures and under pressure. SILCOLAPSE® 426R gives good results at any pH and is particularly effective in alkaline conditions.

Applications:

  • Industrial: Starch production; Adhesive production; Soap and industrial detergent manufacturing; Insecticides, fungicides and pesticides
  • Paper Manufacturing: Wood Pulp Processing; Wash tanks; Glues and pastes
  • Petroleum Refining: Gas scrubbing; Antifreeze additives; Cutting Oil additives; Asphalt production
  • Synthetic Rubber Processing: Natural or synthetic latex
  • Waste Water Treatment
  • Sea Water Distillation
  • Paints, Inks and Varnishes: Manufacture of aqueous pigments in alkaline pH
  • Pesticides
  • Textiles: Sizing and Bleaching; High Temperature Dyeing; Printing; Finishing
Features:
  • Easy to use – as supplied or pre-diluted in water or in the medium to be defoamed
  • Cost efficient, effective in doses as low as 10 ppm
  • Highly effective in most aqueous media, and at all pH levels, especially alkaline
  • Chemically inert in foaming systems – will not alter the properties of the foaming medium
  • Heat resistant – withstands temperatures up to 120°C (248°F)
  • Low viscosity allows it to be used with automatic injection systems

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/cc
pH 6.0
Storage Temperature 5.00 - 40.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
Appearancewhite, creamy liquid
Content30% Active
Diluentswater
Effective Concentrationsfrom 10 ppm
Emulsifier typenonionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
KKPC KOSYN KTR 101 Thermoplastic Elastomer (TPE)
Covestro Bayblock® Base GS Acrylic Basecoat
ChevronTexaco Shingle Oil
American Red Western Cedar (Giant Arborvitae) Wood

PBLUST017 / 190993

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.