MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Vycom FLAMETEC™ CP7-D Flame Retardant Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Flametec™ CP7-D is a proprietary designation for a flame retardant polypropylene formulation. CP7-D represent our version of polypropylene sheet whose flame retardant characteristics meet or exceed the most rigorous FMRC 4910 testing standards for most aspects of flame retardation, self-extinguishing characteristics and burnthrough. In addition, CP7-D also meets or exceeds test standards for low smoke generation and minimal toxic by-products. CP7-D is a filled PP sheet material, therefore, chemical compatibility should be verified for each application.

FEATURES AND BENEFITS

  • Impact Strength- Flexibility and strength of designs vs. other FRPP products.
  • Weldability- Easy to fabricate with conventional welding equipment.
  • Economics- An economical alternative for fire safe construction.
  • Fire Safe- Listed in accordance to FMRC 4910, fire safe materials for clean room construction.
  • Extruded Sheet- Offers the best gauge consistency, surface and tolerances.

Information provided by Compression Polymers Corp - Vycom

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 6710 sec.; ASTM D785
Tensile Strength, Ultimate 2500 psiASTM D638
Elongation at Yield 4.0 %ASTM D638
Flexural Modulus 450000 psiASTM D790
Izod Impact, Notched 10.1 ft-lb/in1/8 in. notch; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 248 °FASTM D648
Vicat Softening Point 299 °F1 kg; ASTM D1525
Flammability, UL94 5VAETL Labs
Flammability Test <= 0.010SDI, FMRC test data; File #3D7Q7.AM
 <= 4.2FPI, FMRC test data; File #3D7Q7.AM
 <= 25(flame) ETL Labs; ASTM E84 Tunnel Test
 <= 100(smoke) ETL Labs; ASTM E84 Tunnel Test
 
Descriptive Properties
Corner Weld Strength, lb/in467CPC Test

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene
E-Polymers TEKAFIN® PH40FR Flame Retardant Heat Resistance Compounded-PP
Vycom FLAMETEC™ CP5 Fire Retardant Polypropylene (FRPP)
Cossa Polimeri ESTAPROP 1540 GFC V0 H Flame Retardant Polypropylene, 20% Glass Filled
Cossa Polimeri ESTAPROP 1050 V0 HF K Flame Retardant Polypropylene

PCPCV04 / 29076

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.