Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.92 g/cc | 1.92 g/cc |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 60 | 60 |
| 46 @Treatment Temp. 200 °C, Time 252000 sec | 46 @Treatment Temp. 392 °F, Time 70.0 hour |
| 53 @Treatment Temp. 200 °C, Time 252000 sec | 53 @Treatment Temp. 392 °F, Time 70.0 hour |
| 57 @Treatment Temp. 150 °C, Time 252000 sec | 57 @Treatment Temp. 302 °F, Time 70.0 hour |
| 57 @Treatment Temp. 23.0 °C, Time 252000 sec | 57 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 57 @Treatment Temp. 100 °C, Time 252000 sec | 57 @Treatment Temp. 212 °F, Time 70.0 hour |
| 59 @Treatment Temp. 150 °C, Time 252000 sec | 59 @Treatment Temp. 302 °F, Time 70.0 hour |
| 60 @Treatment Temp. 23.0 °C, Time 252000 sec | 60 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 60 @Treatment Temp. 250 °C, Time 252000 sec | 60 @Treatment Temp. 482 °F, Time 70.0 hour |
| 62 @Treatment Temp. 275 °C, Time 252000 sec | 62 @Treatment Temp. 527 °F, Time 70.0 hour |
Tensile Strength | 8.984 MPa | 1303 psi |
| 6.360 MPa @Treatment Temp. 275 °C, Time 252000 sec | 922.5 psi @Treatment Temp. 527 °F, Time 70.0 hour |
| 6.666 MPa @Treatment Temp. 200 °C, Time 252000 sec | 966.8 psi @Treatment Temp. 392 °F, Time 70.0 hour |
| 6.9892 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 1013.7 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 7.5822 MPa @Treatment Temp. 200 °C, Time 252000 sec | 1099.7 psi @Treatment Temp. 392 °F, Time 70.0 hour |
| 9.0197 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 1308.2 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 9.0728 MPa @Treatment Temp. 150 °C, Time 252000 sec | 1315.9 psi @Treatment Temp. 302 °F, Time 70.0 hour |
| 9.5320 MPa @Treatment Temp. 250 °C, Time 252000 sec | 1382.5 psi @Treatment Temp. 482 °F, Time 70.0 hour |
| 9.5410 MPa @Treatment Temp. 150 °C, Time 252000 sec | 1383.8 psi @Treatment Temp. 302 °F, Time 70.0 hour |
Elongation, Ultimate | 310 % | 310 % |
| 260 % @Treatment Temp. 23.0 °C, Time 252000 sec | 260 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 279.9 % @Treatment Temp. 200 °C, Time 252000 sec | 279.9 % @Treatment Temp. 392 °F, Time 70.0 hour |
| 300 % @Treatment Temp. 150 °C, Time 252000 sec | 300 % @Treatment Temp. 302 °F, Time 70.0 hour |
| 300.1 % @Treatment Temp. 250 °C, Time 252000 sec | 300.1 % @Treatment Temp. 482 °F, Time 70.0 hour |
| 310 % @Treatment Temp. 150 °C, Time 252000 sec | 310 % @Treatment Temp. 302 °F, Time 70.0 hour |
| 310 % @Treatment Temp. 23.0 °C, Time 252000 sec | 310 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 320 % @Treatment Temp. 200 °C, Time 252000 sec | 320 % @Treatment Temp. 392 °F, Time 70.0 hour |
| 340.1 % @Treatment Temp. 275 °C, Time 252000 sec | 340.1 % @Treatment Temp. 527 °F, Time 70.0 hour |
100% Modulus | 1.58 MPa | 229 psi |
Tear Strength | 21.6 kN/m | 123 pli |
Compression Set | 10.4 % @Treatment Temp. 23.0 °C, Time 79200 sec | 10.4 % @Treatment Temp. 73.4 °F, Time 22.0 hour |
| 10.8 % @Treatment Temp. 175 °C, Time 79200 sec | 10.8 % @Treatment Temp. 347 °F, Time 22.0 hour |
| 13.6 % @Treatment Temp. 200 °C, Time 79200 sec | 13.6 % @Treatment Temp. 392 °F, Time 22.0 hour |
|
Thermal Properties | Metric | English | Comments |
---|
Brittleness Temperature | -25.0 °C | -13.0 °F |
Shrinkage | 0.10 % @Treatment Temp. 23.0 °C, Time 252000 sec | 0.10 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 0.20 % @Treatment Temp. 150 °C, Time 252000 sec | 0.20 % @Treatment Temp. 302 °F, Time 70.0 hour |
| 2.0 % @Treatment Temp. 150 °C, Time 252000 sec | 2.0 % @Treatment Temp. 302 °F, Time 70.0 hour |
| 4.1 % @Treatment Temp. 23.0 °C, Time 252000 sec | 4.1 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 6.0 % @Treatment Temp. 100 °C, Time 252000 sec | 6.0 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 10.5 % @Treatment Temp. 200 °C, Time 252000 sec | 10.5 % @Treatment Temp. 392 °F, Time 70.0 hour |
| 18.8 % @Treatment Temp. 200 °C, Time 252000 sec | 18.8 % @Treatment Temp. 392 °F, Time 70.0 hour |
|
Descriptive Properties |
---|
Color | Brown |