MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Inov Chem Donpanel 415 HFC-365mfc Base blend polyols for PUR
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: DonPanel 415 is a kind of blend polyether polyols with HFC-245fa as foaming agent, taking polyol as the main raw material and mixed with special auxiliary agent. It is suitable for thermal insulation of building boards, cold storage boards and other products. The polyurethane product prepared by reacting it with isocyanate has the following advantages:
-- No greenhouse effect and does not damage the ozone layer
- Good fluidity and uniform foam density
-- Excellent insulation, dimensional stability and adhesion

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 - 1.16 g/cc
Density 0.0240 - 0.0300 g/ccFree density, Manual Mix
 0.0240 - 0.0300 g/ccFree density, High Pressure
 >= 0.0400 g/ccMold density; GB/T 6343
Viscosity 400 - 600 cPDynamic
Storage Temperature 10.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength >= 0.150 MPaGB/T 8813
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity <= 0.0220 W/m-K
@Temperature 10.0 °C
GB/T 3399
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 25.0 °CMaterial Temperature, Manual mix
 20.0 - 25.0 °CMaterial Temperature, High pressure
Cure Time 100 - 240 secTack free time, High pressure
 120 - 280 secTack free time, Manual Mix
Gel Time 1.00 - 2.67 minHigh Pressure
 1.30 - 3.30 minManual Mix
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceLight yellow transparent viscous liquid
Closed-cell rate=90%GB/T 10799
Cream time10-40 secHigh Pressure
 10-50 secManual Mix
Dimensional stability=1.0%24h, -20?; GB/T8811
 =1.5%24h, 100?; GB/T8811
FlammabilityB3GB/T 8624
Hydroxyl value300-400 mgKOH/g
Recommended Ratio100:110-130DonPanel 415:Isocyanate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINOVCHM017 / 312546

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.