MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Non-Black Sulfur Cure
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080
Tensile Strength 20.15 MPa2922 psi
Elongation at Break 671 %671 %
100% Modulus 1.72 MPa
@Strain 100 %
250 psi
@Strain 100 %
200% Modulus 3.01 MPa
@Strain 200 %
436 psi
@Strain 200 %
300% Modulus 5.09 MPa
@Strain 300 %
738 psi
@Strain 300 %
Tear Strength 51.5 kN/m294 pliDie C
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Temperature 155 °C
0.250 hour
@Temperature 311 °F
 
Descriptive Properties
Formulation as Tested0.5Zinc Stearate
 1Thanecure® ZM
 1.5Sulfur
 10Cumar P10
 100Millathane 76
 2AC Poly 617A
 2MBT
 4MBTS
 50Hi-Sil 233

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro DESMODUR® MT2173 + BAYTEC® T20 + BAYTEC® XL B (D1-2 catalyst), 80A Polyurethane, MDI- PTMEG
Northstar Polymers MGB-A80AQ High Performance Polyurethane Cast Elastomer System 80A
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 95A
Northstar Polymers MSS-A80AQ High Performance Polyurethane Cast Elastomer System 80A
Mearthane Durethane™ C 85D Polyurethane

PMILL072 / 87116

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.