MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Versalis SINKRAL D720 ABS, Impact Grade  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Symbol according to ISO 1043-1: ABS

Grade designation according to ISO 2580-ABS 1,MG,095-08-35-15

High impact injection moulding grade, with improved flow compared with SINKRAL B620 and a high gloss. Can be used to mould of helmets as well as in compounds with SAN for the production of 'tailored' ABS grades.

Unfilled. Suitable for Injection Molding. Supplied as pellets. Contains lubricant and release agent.

ISO data. Information provided by Enichem

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³
Water Absorption 1.0 %1.0 %
Moisture Absorption at Equilibrium 0.20 %0.20 %Humidity Absorption
Melt Flow 7.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
cm³/10 min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 34.0 MPa4930 psi50 mm/min
Elongation at Break 20 %20 %Nominal
Elongation at Yield 3.5 %3.5 %50 mm/min
Tensile Modulus 1.70 GPa247 ksi1 mm/min
Charpy Impact Unnotched NBNB
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Charpy Impact, Notched 3.00 J/cm²14.3 ft-lb/in²
 1.90 J/cm²
@Temperature -30.0 °C
9.04 ft-lb/in²
@Temperature -22.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm1.00e+14 ohm
Dielectric Constant  2.7
@Frequency 100 Hz
2.7
@Frequency 100 Hz
 3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
Dielectric Strength 30.0 kV/mm762 kV/in
Dissipation Factor  0.0065
@Frequency 1e+6 Hz
0.0065
@Frequency 1e+6 Hz
 0.0090
@Frequency 100 Hz
0.0090
@Frequency 100 Hz
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature 20.0 °C
50.0 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °F
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C169 °F
Vicat Softening Point 94.0 °C201 °F50°C/hr; 50N
Glass Transition Temp, Tg 105 °C221 °F10°C/min test
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.10 mm
HB
@Thickness 0.122 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Diamond ABS 3500 HF Injection Molding Grade, High Flow, Medium Impact
Elix Polymers ELIX ABS P2M-AT Acrylonitrile Butadiene Styrene (ABS), High Impact Strength
Stratasys® ABS
A. Schulman Diamond ABS 3501
A. Schulman Diamond ABS 3500ELG

PENJ81 / 35952

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.