MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Sumitomo Bakelite 52-70-70 V0-P Diallyl Phthalate Compound
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled

Material Notes: 52-70-70 V0-P is a glass fiber reinforced diallyl phthalate compound which conforms with the requirements of ASTM D5948 Type SDG-F.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.91 g/cc1.91 g/ccASTM D792
Apparent Bulk Density 0.750 g/cc0.0271 lb/in³Powder; ASTM D1895
Water Absorption 0.25 %
@Time 173000 sec
0.25 %
@Time 48.0 hour
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 75.0 MPa10900 psiASTM D638
Flexural Strength 124 MPa18000 psiASTM D790
Flexural Modulus 11.7 GPa1700 ksiASTM D790
Compressive Strength 150 MPa21800 psiASTM D695
Izod Impact, Notched 0.320 J/cm0.599 ft-lb/inASTM D256A
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
wet; ASTM D150
Dielectric Strength >= 13.8 kV/mm
@Frequency 60 Hz
>= 351 kV/in
@Frequency 60 Hz
SS, wet
Dissipation Factor 0.014
@Frequency 1e+6 Hz
0.014
@Frequency 1e+6 Hz
wet; ASTM D150
Arc Resistance 130 sec130 secASTM D495
Comparative Tracking Index >= 600 V>= 600 VTracking Resistance; ASTM D3635
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 130 °C266 °FUL 746B Temperature Index
Deflection Temperature at 1.8 MPa (264 psi) >= 280 °C>= 536 °FAs Molded; ASTM D648A
 >= 280 °C>= 536 °FPost Baked; ASTM D648A
Flammability, UL94  V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSUMIT124 / 193929

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.