MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECATOR™ TI 5031 Polyamide-imide (PAI), Bearing Grade
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI)

Material Notes: TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger are available in three grades: TECATOR™ TI 5013, high strength structural grade featuring good electrical properties and strength, making it ideal for demanding applications at a broad range of temperatures. TECATOR™ TI 5031 offers high PV capabilities in bearing applications, primarily at high loads and low speeds. TECATOR™ GF30 (XP1424T) is a 30% glass filled grade, compression molded with superior stiffness and dimensional stability. It is available in a wide variety of custom tube, ring, rod and plate sizes.

  • Excellent weather and gamma radiation resistance
  • Outstanding bearing wear properties (at elevated temperatures, TECATOR™ TI 5031 offers superior wear rates)
  • High strength and stiffness
  • Excellent electrical values
  • Good chemical resistance (TECATOR™ is not attacked by common solvents or fuels and is acceptable for use in contact with many acids)
  • Maintains a high proportion of mechanical properties over a broad temperature spectrum - cryogenic to 500°F
  • TECATOR™ TI 5013 and TI 5031 are available in a wide variety of metric sizes in rod and plate

TECATOR™ (PAI) typical applications: Pump parts, valve seats, piston rings, seal rings, engine transmission parts and bearing cages. For the semiconductor industry it is used for "burn in" test sockets, nests, chassis and other applications such as welding nozzle tips.

Information Provided by Ensinger Industries, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.46 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 109ASTM D785
Tensile Strength at Break 19000 psi
@Temperature 22.8 °C
ASTM D638
Elongation at Break 10 %
@Temperature 22.8 °C
ASTM D638
Flexural Strength 23000 psi
@Temperature 22.8 °C
ASTM D790
Flexural Modulus 870000 psi
@Temperature 22.8 °C
ASTM D790
Izod Impact, Notched 2.00 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.8
@Frequency 2.00e+7 Hz
ASTM D150
 3.9
@Frequency 3.00e+7 Hz
ASTM D150
Dissipation Factor 0.012
@Frequency 2.00e+7 Hz
 0.018
@Frequency 3.00e+7 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °Fcontinuous
Deflection Temperature at 1.8 MPa (264 psi) 534 °FASTM D648
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger TECATOR™ TI 5013 Polyamide-imide (PAI)
Ensinger TECATOR™ GF30 (XP142T) Polyamide-imide (PAI), 30% glass filled, compression molded
ATI Allegheny Ludlum Grade 5 Titanium 6Al-4V (UNS R56400)
Hippe PAI Polyamide-imide
Isoflon PAI Polyamideimide

PENSIN033 / 92850

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.