MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Asahi Kasei Leona™ 90G33 Polyamide 66, GF Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Enhanced strength and stiffness; with 33% GF. Superior fluidity and appearance.

Applications:Automotive parts

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/ccDry as Molded; ASTM D792
Density 1.39 g/ccDry as Molded; ISO 1183
Moisture Absorption at Equilibrium 1.4 %
@Temperature 23.0 °C
50% RH; ISO 62
 1.4 %
@Temperature 23.0 °C
50% RH
Linear Mold Shrinkage, Flow >= 0.0040 cm/cmAsahi Kasei
Linear Mold Shrinkage, Transverse >= 0.0090 cm/cmAsahi Kasei
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 90Dry as Molded; ISO 2039
Hardness, Rockwell R 120Dry as Molded; ISO 2039
Tensile Strength at Break 150 MPaConditioned at 50% RH; ISO 527
 180 MPaDry as Molded; ISO 527
Tensile Strength 157 MPaConditioned at 50% RH; ASTM D638
 194 MPaDry as Molded; ASTM D638
Elongation at Break 2.5 %Dry as Molded; ISO 527
 3.0 %Conditioned at 50% RH; ISO 527
Tensile Modulus 9300 MPaConditioned at 50% RH; ISO 527
 10200 MPaDry as Molded; ISO 527
Flexural Strength 216 MPaConditioned at 50% RH; ISO 178
 238 MPaDry as Molded; ISO 178
Flexural Modulus 8100 MPaConditioned at 50% RH; ISO 178
 10000 MPaDry as Molded; ISO 178
Izod Impact, Notched 98.0 J/mDry as Molded; ASTM D256
 118 J/mConditioned at 50% RH; ASTM D256
Charpy Impact Unnotched 54.0 kJ/m²Conditioned at 50% RH; ISO 179
 55.0 kJ/m²Dry as Molded; ISO 179
Charpy Impact, Notched 6.00 kJ/m²Dry as Molded; ISO 179
 12.0 kJ/m²Conditioned at 50% RH; ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°CDry as Molded; ASTMD 696
Deflection Temperature at 0.46 MPa (66 psi) 235 °CDry as Molded; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 220 °CDry as Molded; ISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asahi Kasei Leona™ 13G25 Polyamide 66, GF Reinforced
Asahi Kasei Leona™ 54G33 Polyamide 66, GF Reinforced
Asahi Kasei Leona™ 13G15 Polyamide 66, GF Reinforced
Asahi Kasei Leona™ 13G50 Polyamide 66, GF Reinforced
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Filled

PASAHI8141 / 221168

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.