MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay FM® 410 Adhesive Foam
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: FM® 410 adhesive foam, a modified epoxy material, is supplied in sheet form and may be cured in place by either a free-foaming or restrained foaming process. The operating temperature is -67°F to 350°F (-55°C to 177°C). FM 410 is specifically designed for splicing honeycomb core under ambient pressure. Typical applications are bonding of inserts or edge members to core and local honeycomb core reinforcement where increased shear strength is required. Because FM 410 contains no metallic fillers it has good radar transparency.

Features & Benefits:

  • Designed for splicing honeycomb core under ambient pressure
  • Bonds inserts or edge members to honeycomb core
  • No metallic filler or asbestos
  • Provides local honeycomb core reinforcement where increased shear is required
  • Cure temperature 225°F to 350°F (107°C to 177°C)
Applications:
  • Splicing honeycomb core
  • Bonding of inserts or edge members to core
  • Local reinforcement of honeycomb core

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.320 - 0.641 g/cc
Volatiles <= 1.0 %
Storage Temperature <= -18.0 °C
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 715 psiTube, 177°C Cure, Tested at 75°F (24°C) after 3 days water boil
 841 psiTube, 177°C Cure, Tested at 75°F (24°C) after 7 days immersion in Skydrol at 150°F (66°C)
 846 psiTube, 121°C Cure, Tested at 75°F (24°C) after 7 days immersion in Skydrol at 150°F (66°C)
 905 psiTube, 121°C Cure, Tested at 75°F (24°C) after 15 minutes trichloroethylene degreasing and 30 minute post bake at 250°F (121°C)
 905 psiTube, 177°C Cure, Tested at 75°F (24°C) after 15 minutes trichloroethylene degreasing and 30 minute post bake at 250°F (121°C)
 950 psiTube, 121°C Cure, Tested at 75°F (24°C) after 3 days water boil
 1072 psiTube, 177°C Cure, Tested at 75°F (24°C) after 30 days salt spray at 95°F (35°C)
 1211 psiTube, 121°C Cure, Tested at 75°F (24°C) after 30 days salt spray at 95°F (35°C)
 130 psi
@Temperature 177 °C
Tube, 177°C Cure
 755 psi
@Temperature 121 °C
Tube, 121°C Cure
 755 psi
@Temperature 121 °C
Tube, 177°C Cure
 825 psi
@Temperature 24.0 °C
Tube, 177°C Cure
 915 psi
@Temperature 24.0 °C
Tube, 121°C Cure
 945 psi
@Temperature -55.0 °C
Tube, 177°C Cure
 975 psi
@Temperature -55.0 °C
Tube, 121°C Cure
 1000 psi
@Temperature 82.0 °C
Tube, 121°C Cure
 1010 psi
@Temperature 82.0 °C
Tube, 177°C Cure
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 177 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
ColorBlue turning green during cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay FM® 410-1 Core Splice Foam

PCYTED037 / 180339

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.