MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ExxonMobil Exterex™ TM111 Synthetic Fluid
Categories: Fluid; Lubricant

Material Notes: Product Description: Esterex™ Tirmellitate Esters are API category Group V fluids. These esters have excellent low-temperature properties, good lubricating properties and low volatilities. Esterex™ Trimellitate Esters can be used as sole basestocks or blendstocks with other synthetic fluids in many engine and industrial lubricant applications.

Appearance: Bright & Clear

Availability: Asia Pacific, Central America, North America and South America

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.978 g/cc
@Temperature 15.6 °C
0.0353 lb/in³
@Temperature 60.1 °F
ASTM D4052
Viscosity Measurement 8181Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 124 cSt124 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 11.9 cSt11.9 cStASTM D445
Evaporation Loss 1.0 %
@Temperature 205 °C,
Time 23400 sec
1.0 %
@Temperature 401 °F,
Time 6.50 hour
ASTM D972
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.16<= 0.16[mg KOH/g]; ASTM D974 (mod)
 
Thermal PropertiesMetricEnglishComments
Pour Point -32.8 °C-27.0 °FASTM D5950/D97
Flash Point 240 °C464 °FPMCC; ASTM D92
 274 °C525 °FCOC; ASTM D92
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.48451.4845ASTM D1218
 
Descriptive Properties
Aniline Point16.5°FASTM D611
Biodegradation<1%OECD 301F
Color<0.5ASTM D1500
CompositionWater<1000 ppm, ASTM D6304 (mod)
Density Correction Factor0.000733 (g/cc)/°CASTM D1250
Elastomer Compatibility (%)-0.5Nitrile Tensile Strength Change, ASTM D471
 -10Nitrile Hardness Change, ASTM D471
 14.5Nitrile Volume Change, ASTM D471
 15.1Polyacrylate Elongation Change, ASTM D471
 -16Polyacrylate Hardness Change, ASTM D471
 18.1Polyacrylate Volume Change, ASTM D471
 -18.8Nitrile Elongation Change, ASTM D471
 2.3Fluoroelastomer Volume Change, ASTM D471
 -20.7Fluoroelastomer Tensile Strength Change, ASTM D471
 -24.3Polyacrylate Tensile Strength Change, ASTM D471
 -3Fluoroelastomer Hardness Change, ASTM D471
 9.2Fluoroelastomer Elongation Change, ASTM D471
Fire Point576°FCOC, ASTM D92
Hydrolytic Stability, TAN Change0.01 mg KOH/gASTM D2619
Kauri-Butanol Value35ASTM D1133
Noack Volatility (%)1.4ASTM D5800/DIN 51581
RPVOT>1210 minWith AO, ASTM D2272
 310 minNeat, ASTM D2272

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEX99707 / 175943

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.