MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Adflex Q 109 F Thermoplastic Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Adflex Q 109 F is a reactor TPO (thermoplastic polyolefin) manufactured using Lyondell Basell's proprietary Catalloy process technology. It is suitable for the extrusion and calendering of soft film and sheet, for the impact modification of polypropylene and other compounding applications, as well as monolayer and multilayer air quenched blown films. It is also used by our customers for automotive color-matched interior trim applications. The grade is available in natural pellet form and has no slip or antiblock, and contains a unique stabilization package for color sensitive applications. Additional suitable stabilization is recommended to protect the resin during melt processing and throughout its useful life.

Availability: Asia-Pacific; North America; South & Central America

Application: Bags & Pouches; Interior Automotive Applications; Soft Profile & Sheets; Specialty Film; TPO Foils and Skins

Market: Automotive; Flexible Packaging

Processing Method: Blown Film; Calendaring; Extrusion Flat-die; Sheet; Thermoforming

Attribute: Good Colorability; Good Flexibility; Good Impact Resistance; Good Puncture Resistance; High ESCR (Environmental Stress Cracking Resistance); Low Gloss; Low Hardness; Medium Heat Resistance

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³Method A; ISO 1183-1
Melt Flow 0.600 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.600 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 30.0
@Time 15.0 sec
30.0
@Time 0.00417 hour
ISO 868
Tensile Strength at Break 10.0 MPa1450 psiISO 527-1, -2
Elongation at Break 500 %500 %ISO 527-1, -2
Flexural Modulus 0.100 GPa14.5 ksiISO 178
Charpy Impact, Notched  0.280 J/cm²
@Temperature -40.0 °C
1.33 ft-lb/in²
@Temperature -40.0 °F
Complete Break; ISO 179
 4.10 J/cm²
@Temperature 23.0 °C
19.5 ft-lb/in²
@Temperature 73.4 °F
Partial Break; ISO 179
 10.7 J/cm²
@Temperature -20.0 °C
50.9 ft-lb/in²
@Temperature -4.00 °F
Partial Break; ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 142 °C288 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 40.0 °C104 °FUnannealed; ISO 75B-1, -2
Vicat Softening Point 60.0 °C140 °FA/50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze  9.00 %
@Thickness 0.0500 mm
9.00 %
@Thickness 0.00197 in
ASTM D1003
 47.0 %
@Thickness 1.14 mm
47.0 %
@Thickness 0.0450 in
ASTM D1003
Gloss  50.0 %
@Thickness 0.0500 mm
50.0 %
@Thickness 0.00197 in
45°; ASTM D2457
 87.0 %
@Thickness 1.14 mm
87.0 %
@Thickness 0.0450 in
60°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9005 / 323933

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.