MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene® LP510300 High Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes:

Applications
PETROTHENE LLP 5103-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good drawdown. It is recommended for merchandise bags, and multi-wall sack liners and barrier sheeting. It is also useful as a blend component for improved stiffness and machineability.

Regulatory Status
LP 5103-00 meets the requirements of Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Processing Techniques
Specific recommendations for processing LP 5103-00 can only be made when the processing conditions, equipment and end use are known.

The physical properties are typical values and are not to be construed as specific product limits. Film properties obtained on 1.25 mil film produced using a 2.2:1 blow-up ratio.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.949 g/ccASTM D1505
Water Vapor Transmission 6.60 g/m²/dayASTM F372
Oxygen Transmission Rate 2900 cc/m²/dayASTM D3985
Thickness 1.25 mil2.2:1 BUR
Melt Flow 0.33 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 450 %ASTM D882
Film Elongation at Break, TD 600 %ASTM D882
Dart Drop Test 40.0 gASTM D1709
Film Tensile Strength at Break, MD 8000 psiASTM D882
Film Tensile Strength at Break, TD 3800 psiASTM D882
1% Secant Modulus, MD 112000 psi1% Secant; ASTM D882
1% Secant Modulus, TD 160000 psi1% Secant; ASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 126 °CASTM D1525
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 9656 HDPE Blown Film Resin
Chevron Phillips Marlex® 7109DL LLDPE Blown Film Resin
LyondellBasell Petrothene® LP510300 High Density Polyethylene, Film Extrusion Data
Braskem HF 0150 HDPE Blown Film Extrusion Polyethylene
Overview of materials for High Density Polyethylene (HDPE), Injection Molded

PEQU0169 / 36599

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.