Description/Features: - UL Recognized 720 hr. Sunlight Resistant Jacket per UL QMTT2
- UL 105°C
- UL 62 Class 12, Class 43
- SJT
- SPT Cord
Applications: - Apparatus & Cord Jacket
- Apparatus & Cord Insulation
Market: Processing Method: PolyOne First ChoiceDisclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation. Geon Performance Solutions was created from PolyOne in 2019. |