MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo Magnum™ FG960 ABS, High Impact  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

Material Notes: MAGNUM ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resins are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming.

MAGNUM PG914 and FG960 ABS resins are specifically designated for use as pipe and fittings for Drain, Waste and Vent applications which meet ASTM D-2661 DWV, D2750 Conduit, D2751 Sewer, F-480 Well Casing and F-628 Cellular Core DWV standards. MAGNUM PG960 and FG914 are listed under standard 14 of the National Sanitation Foundation.

MAGNUM FG960 ABS resin is a low gloss, high impact strength resin. Sold as prime, virgin material, it is injection molded directly into pipe fittings for the drain, waste and vent markets. MAGNUM FG960 is available in clack as a factory color mix product (natural resin with black color concentrate), designated No. 21050-Black-7.

Data provided by Dow Chemical.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM Data
Linear Mold Shrinkage 0.0055 cm/cm0.0055 in/in
Melt Flow 2.6 g/10 min
@Load 3.80 kg,
Temperature 230 °C
2.6 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM Data
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 104104
Tensile Strength, Ultimate 35.9 MPa5210 psiASTM Data
Tensile Strength, Yield 37.2 MPa5400 psiASTM Data
Elongation at Break 70 %70 %ASTM Data
Elongation at Yield 2.6 %2.6 %ISO Data
Tensile Modulus 1.86 GPa270 ksiASTM Data
Izod Impact, Notched 2.46 J/cm4.61 ft-lb/inASTM Data
Charpy Impact Unnotched NBNBISO Data
 NBNBISO Data, Low Temp
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO Data, Low Temp
 2.20 J/cm²10.5 ft-lb/in²ISO Data
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 79.0 µm/m-°C
@Temperature 20.0 °C
43.9 µin/in-°F
@Temperature 68.0 °F
ISO data
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C170 °FUnannealed; 101°C (214°F) annealed; ASTM Data
Vicat Softening Point 105 °C221 °F
 
Optical PropertiesMetricEnglishComments
Gloss 40 %40 %Gardner Gloss, 60°

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo Magnum™ 9020 ABS, High Gloss
Trinseo Magnum™ 9010 ABS, High Gloss
Trinseo Magnum™ 9030 ABS, High Gloss
Covestro Makrolon® 1143 Polycarbonate
Covestro Makroblend® UT-640 G Polycarbonate + Polyester Blend

PZZDW115 / 34346

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.