MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
North American Engelmann Spruce Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Softwood with resin canals. Data is based on small, clear, air-dried samples unless specified.

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Picea engelmannii; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.350 g/ccAir Dry (12-15% Moisture Content)
Cell Length 3.00 mmMature Wood
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 1700 NSide
Tensile Strength, Ultimate 2.40 MPaPerpendicular to Grain
 88.0 MPaAxial
Modulus of Rupture 0.0640 GPaStatic Bending
 4.20 ksiStatic Bending*
Flexural Yield Strength 2500 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 8.90 GPaStatic Bending
Compressive Strength 2.80 MPaPerpendicular to Grain
 31.0 MPaParallel to Grain
 290 psiPerpendicular to Grain*
 1740 psiParallel to Grain*
 1980 psiMax Crushing Strength Parallel to Grain*
Poissons Ratio 0.058µTL, 12% Moisture Content
 0.083µRL, 12% Moisture Content
 0.255µTR, 12% Moisture Content
 0.422µLR, 12% Moisture Content
 0.462µLT, 12% Moisture Content
 0.53µRT, 12% Moisture Content
Shear Strength 8.30 MPaOrientation Unknown
 590 psiParallel to Grain*
Toughness 12.5 JRadial
 20.4 JTangential
Cleavage 19.0 kN/mRadial surface of failure, Unseasoned*
 24.0 kN/mTangential surface of failure, Unseasoned*
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.630 BTU-in/hr-ft²-°FOven Dry
 0.750 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 3.4 %Radial; Green to Zero Moisture
 6.6 %Tangential; Green to Zero Moisture
 10.4 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Red Spruce Wood
Canadian Spruce Wood
American Balsam Fir Wood
North American Quaking Aspen (Trembling Aspen) Wood
American White Spruce Wood

PTSA120 / 71250

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.