MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vikas Ecotech Vikoflex VF-09C PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Product Description: Vikoflex range of PVC Compounds are designed precisely as per application needs & manufactured on the latest, high end machines, matching international standards. We offer products of high consistency in the quality & performance, meeting varied needs like high fire retardance, low smoke emissions, high strength, heavy metal free & non toxic compounds for a host of applications like cable insulation, pressure pipes, hydraulics hoses, fittings, footwear & many more.

Characteristics & Usages:

  • Chemically Inert
  • High strength to weight ratio.
  • Tough and dent resistant.
  • An electrical and thermal insulator.
  • Water, Corrosion and Weather resistant.
Applications: Heat Resistant up to 105°C

Information provided by Vikas Ecotech LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 - 1.34 g/cc1.30 - 1.34 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 92 - 9692 - 96ASTM D2240
Tensile Strength >= 20.5 MPa>= 2970 psiIS 10810
Elongation at Break >= 200 %>= 200 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 5.00e+14 ohm-cm>= 5.00e+14 ohm-cmIS 3396
 
Descriptive Properties
Thermal Stability>130 minutesat 200°C, IS 5831

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PVICAS029 / 285442

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.