MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Reynolds PMC® 780 Dry & Wet Industrial Liquid Rubber Compound
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: Product Overview: PMC-780 is a premium performance urethane rubber that offers exceptional strength, durability and abrasion resistance. PMC-780 DOES NOT CONTAIN MOCA – a known cancer causing agent and hazard. Mixed two parts A to one part B by weight or volume, PMC-780 urethane pours easily and cures at room temperature with negligible shrinkage to a solid Shore 80A rubber. Pick The One Best Suited For Your Application: Original PMC-780 Dry does not exude oil. New PMC-780 Wet contains a built in release agent to aid in demolding concrete. (Note: “wet” rubber has a higher net shrinkage value over time vs. “dry “ rubber.) Both are used around the world for casting abrasive materials such as concrete (pre-cast concrete, making concrete stamping pads, etc.) and gypsum plasters with high exotherms. PMC-780 Dry is also commonly used to make rubber mechanical parts of varying configurations (gaskets, wheels, and pullies) as well as ball mill liners and vibration/shock pads.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccASTM D-1475
Viscosity 2000 cP2000 cPMixed; ASTM D-2393
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D-2240
Tensile Strength 6.21 MPa900 psiASTM D-412
Elongation at Break 700 %700 %ASTM D-412
100% Modulus 2.76 MPa400 psiASTM D-412
Tear Strength 35.1 kN/m200 pliDie C; ASTM D-624
 
Processing PropertiesMetricEnglishComments
Cure Time 2880 min48.0 hour
Pot Life 25.0 min25.0 minASTM D-2471
 
Descriptive Properties
ColorLight Amber
Mix Ratio2A:1Bby volume
 2A:1Bby weight
Specific Volume27.2[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN080 / 296781

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.