MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Momentive Performance Materials TSE3282-G Thermally Conductive Silicone Adhesive  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Elastomer, for Thermal Management

Material Notes: TSE328-G silicone adhesive is a one-component, low viscosity, thermally conductive material, which will remain in an uncured state at room temperature and cure to an elastomer when heat is applied.

TSE3282-G provides much higher thermal conductivity than conventional silicone adhesives, which makes it ideal for electrical and electronic applications where high thermal transfer is required. it is non-corrosive to metals and has excellent adhesive properties to a wide variety of substrates, generally without the need for using a primer. For example, primerless adhesion is typically obtained on metals such as aluminum, copper, and nickel plate, PPS and PBT plastics, ceramics, and glass.

Cured properties for specimen cured for 1 hour at 150°C.

Key Performance Properties:

  • Excellent thermal conductivity
  • Ready to use - once component
  • Heat accelerated cure
  • Excellent adhesive properties; this material offers primerless adhesion to many substrates
  • Non corrosive to metals

GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.70 g/cc
@Temperature 23.0 °C
Viscosity 20000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
Tensile Strength at Break 4.00 MPa
Elongation at Break 50 %
Adhesive Bond Strength 363 psiAluminum lap shear
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.80e+14 ohm-cm
Dielectric Constant 5.5
@Frequency 60 Hz
Dielectric Strength 23.0 kV/mm
Dissipation Factor 0.0010
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 140 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 2.00 W/m-K
 
Descriptive Properties
ColorGray
ConsistencyFlowable paste

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials TSE3280G Thermally Conductive, Heat Cured Silicone Adhesive
Momentive Performance Materials TSE3281G Thermally Conductive, Heat Cured Silicone Adhesive
Momentive Performance Materials TSE392 One Component RTV Adhesive Sealant/Coating, Clear/White
Momentive Performance Materials TSE397 One Component RTV Adhesive Sealant/Coating, Clear/White
Master Bond Mastersil 705TC One Component, Thermally Conductive Silicone

PGESIL071 / 41062

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.