MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes:

Applications: Easy-Flo is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wetting and bonding. In brazing gray cast iron it is necessary to treat the surface prior to brazing to remove graphite, in order to assure good wetting by the brazing filler metal.

A complete list of the uses of Easy-Flo would include practically all applications for which silver brazing filler metals have been used.

Characteristics:Easy-Flo is a are eutectic type, free-flowing filler metals that, because of their narrow melting range, are less sensitive to the rate of heating and should not liquate (i.e. separate into low and high melting constituents). This high fluidity makes well-fitted joints essential and prevents bridging or large fillet formation. Handy Flux should be used with either of these filler metals.

Some base metals when brazed under high stress may crack during brazing when the stressed base metal is wetted by the brazing filler metal. This is a form of stress corrosion cracking. The low flow temperature of Easy-Flo is below the stress relaxation temperature of some nickel base alloys. The cure is to relieve the stress before the brazing alloy is applied. A higher melting brazing filler metal may be preferred since stress relief will then occur before the filler metal melts.

Specifications:This filler metal conform to the following specifications: AWS A5.8 BAg-1a, SAE-AMS 4770, ASME Boiler and Pressure Vessel Code Section II-C SFA 5.8 BAg-1a

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 9.45 g/cc0.341 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 379 MPa55000 psiArmco Iron (0.05% C) butt joint
 414 MPa60000 psiStainless Steel (18-8) Annealed butt joint
 448 MPa65000 psi1020 Steel butt joint
 586 MPa85000 psi1095 (Drill Rod) butt joint
 621 MPa90000 psiHigh Speed Steel (18 W, 4 Cr, 1 V) butt joint
 758 MPa110000 psi4140 Steel butt joint
 896 MPa130000 psiStainless Steel 918-8) Cold Rolled butt joint
 55.2 MPa
@Temperature 482 °C
8000 psi
@Temperature 900 °F
Inconel butt joint
 82.7 MPa
@Temperature 427 °C
12000 psi
@Temperature 800 °F
Stainless Steel (18-8) butt joint
 89.6 MPa
@Temperature 482 °C
13000 psi
@Temperature 900 °F
Monel butt joint
 262 MPa
@Temperature 260 °C
38000 psi
@Temperature 500 °F
Inconel butt joint
 310 MPa
@Temperature 23.0 °C
45000 psi
@Temperature 73.4 °F
 331 MPa
@Temperature 260 °C
48000 psi
@Temperature 500 °F
Monel butt joint
 338 MPa
@Temperature 260 °C
49000 psi
@Temperature 500 °F
Stainless Steel (18-8) butt joint
 483 MPa
@Temperature 23.0 °C
70000 psi
@Temperature 73.4 °F
 696 MPa
@Temperature 23.0 °C
101000 psi
@Temperature 73.4 °F
Elongation at Break  0.00 %
@Temperature 260 °C
0.00 %
@Temperature 500 °F
in 2", Stainless Steel (18-8) butt joint
 0.00 %
@Temperature 260 °C
0.00 %
@Temperature 500 °F
in 2", Inconel butt joint
 0.00 %
@Temperature 427 °C
0.00 %
@Temperature 800 °F
in 2", Stainless Steel (18-8) butt joint
 0.00 %
@Temperature 482 °C
0.00 %
@Temperature 900 °F
in 2", Inconel butt joint
 0.00 %
@Temperature 482 °C
0.00 %
@Temperature 900 °F
in 2", Monel butt joint
 0.00 %
@Temperature 23.0 °C
0.00 %
@Temperature 73.4 °F
 0.00 %
@Temperature 23.0 °C
0.00 %
@Temperature 73.4 °F
 3.1 %
@Temperature 260 °C
3.1 %
@Temperature 500 °F
in 2", Monel butt joint
 7.3 %
@Temperature 23.0 °C
7.3 %
@Temperature 73.4 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000700 ohm-cm0.00000700 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Melting Point 627 - 635.0 °C1160 - 1175 °F
Solidus 627 °C1160 °FMelting Point
Liquidus 635.0 °C1175 °FFlow Point
 
Processing PropertiesMetricEnglishComments
Processing Temperature 635.0 - 746.1 °C1175 - 1375 °FBrazing Range
 
Component Elements PropertiesMetricEnglishComments
Cadmium, Cd 17 - 19 %17 - 19 %
Copper, Cu 14.5 - 16.5 %14.5 - 16.5 %
Other, total <= 0.15 %<= 0.15 %
Silver, Ag 49 - 51 %49 - 51 %
Zinc, Zn 14.5 - 18.5 %14.5 - 18.5 %
 
Descriptive Properties
ColorLight Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
Lucas-Milhaupt Cerametil 616 Active Metal Brazing
Lucas-Milhaupt EASY FLO 45 Silver Based Cadmium-Bearing Filler Metal
AISI 1141 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 4118H Steel, annealed at 870°C (1600°F), furnace cooled at 11°C (20°F)/hour, 25 mm (1 in.) round

NLUCMI43 / 18110

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.