MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kraiburg TPE THERMOLAST® K TC6PAZ Thermoplastic Elastomer (AD/PA Series) Adhesion to PA
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The AD/PA series is a material solution for applications with adhesion to PA. The compounds are available in black and natural colors. Natural color variants can be colored in many different ways.

Processing Method: Injection Molding

Color / RAL DESIGN:

  • Natural
  • Black
Typical applications:
  • Thumb wheels
  • Function and design elements
  • Handles (tools and power tools, etc.)
  • Grommets
  • Cable clips
Material advantages:
  • Adhesion to PA6 and PA6.6, up to 50% glass fiber
  • Adhesion to PA12
  • Halogen-free (according to IEC 61249-2-21)
  • Dry haptics
  • Colorable
  • Temperature stability up to 90 °C

Information provided by Kraiburg TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³DIN EN ISO 1183-1
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5858DIN ISO 48-4
Tensile Strength 3.00 MPa435 psi200 mm/min; DIN 53504/ISO 37
Elongation at Break 400 %400 %200 mm/min; DIN 53504/ISO 37
Tear Strength 16.0 kN/m91.3 pliISO 34-1 Method B (b)
 
Descriptive Properties
Adhesion to PA65.5 N/mm (D)VDI 2019 two-component injection
Adhesion to PA6.64.0 N/mm (B/D)VDI 2019 two-component injection
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKRAIA8009 / 308673

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.