MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess Antilux® 654 L Wax
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Anti-check wax to protect rubber articles against cracking caused by ozone and weathering influences

Use: Owing to its reduced solubility, Antilux 654 L migrates to the surface of the vulcanizates where it forms a complete protective film which remains stable at temperatures up to about 50 °C. The formation of the film takes place at a medium-fast rate. The film shows an excellent stability against dynamic stress. Antiozonants and antioxidants are carried to the surface of the vulcanizate by the migration of Antilux 654 L. The technological effect is comparable to the one of Antilux 654.

Application: Rubber articles which come into contact with foodstuffs, toys, surgical and pharmaceutical rubber articles

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.5 Month
@Temperature <=35.0 °C
36.5 Month
@Temperature <=95.0 °F
 
Descriptive Properties
Appearancewhite Pellets
Specifications64-66°CCongealing point, ISO 2207

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8265 / 208658

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.