KEBALLOY ECO FE 220104 PPS is an unfilled PPS recyclate. Properties: dimensionally stable, good aging behavior, good fire behavior, high continuous used temperature, High strength, semi-crystalline Typical areas of application: Covers, Cover, Electronic components, Housing, Lamp socket, Cables and connectors for media-carrying systems, Pump housing, Sensors, Bobbin, Plug, Valves, Valve caps, Distributor Industries: Automotive, Electrical and electronics industry, Household appliances, Industry Information provided by BARLOG plastics GmbH. |