MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Abatron AboCast/AboCure 8109-1
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: High melting point.

Processing: 100/30 pbw; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°F).

Applications: Heavy duty casting and potting.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³
Water Absorption 0.25 - 0.35 %0.25 - 0.35 %(60x10X4 mm bar) after 10 days at 20°C (77°F)
 0.30 - 0.45 %0.30 - 0.45 %(60x10X4 mm bar) after 1 hour at 100°C (212°F)
Viscosity 200 - 600 cP
@Temperature 120 °C
200 - 600 cP
@Temperature 248 °F
Vapor Pressure  <= 0.0000133 bar
@Temperature 20.0 °C
<= 0.0100 torr
@Temperature 68.0 °F
AboCure
 <= 0.00133 bar
@Temperature 180 °C
<= 1.00 torr
@Temperature 356 °F
AboCast
 0.00133 bar
@Temperature 100 °C
1.00 torr
@Temperature 212 °F
AboCure
 0.00373 bar
@Temperature 120 °C
2.80 torr
@Temperature 248 °F
AboCure
 0.0133 bar
@Temperature 135 °C
10.0 torr
@Temperature 275 °F
AboCure
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 82.73 MPa12000 psi
Modulus of Elasticity 2.758 GPa400.0 ksi
Flexural Yield Strength 137.9 MPa20000 psi
Compressive Yield Strength 117.2 MPa17000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.50e+16 ohm-cm>= 1.50e+16 ohm-cm
Dielectric Constant  3.5 - 3.7
@Frequency 1000 Hz
3.5 - 3.7
@Frequency 1000 Hz
 3.5 - 3.7
@Frequency 1e+6 Hz
3.5 - 3.7
@Frequency 1e+6 Hz
 3.6 - 3.9
@Frequency 50 Hz
3.6 - 3.9
@Frequency 50 Hz
Dielectric Strength 14.76 - 17.72 kV/mm
@Thickness 3.17 mm
374.9 - 450.1 kV/in
@Thickness 0.125 in
Short time value
Dissipation Factor  0.0030 - 0.0070
@Frequency 50 Hz
0.0030 - 0.0070
@Frequency 50 Hz
 0.0050 - 0.010
@Frequency 1000 Hz
0.0050 - 0.010
@Frequency 1000 Hz
 0.025 - 0.035
@Frequency 1e+6 Hz
0.025 - 0.035
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 - 65.0 µm/m-°C
@Temperature 20.0 °C
33.3 - 36.1 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.170 - 0.200 W/m-K1.18 - 1.39 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 110 °C230 °FDeflection temperature; load unknown.
 
Processing PropertiesMetricEnglishComments
Processing Temperature 130 - 140 °C266 - 284 °F
Pot Life 90.0 min
@Temperature 120 °C
90.0 min
@Temperature 248 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arlon Electronic Materials 45N Multifunctional Epoxy Laminate and Prepreg
Atom Adhesives AA-BOND F110 Epoxy Adhesive
Overview of materials for Epoxy Adhesive
Abatron AboCoat 8204-15/AboCure 8204-15 Epoxy Coating
Abatron AboCast/AboCure 8502-1 Epoxy

PABEP1 / 22015

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.