MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem INSPIRE™ 404 Performance Polypropylene Polymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Sheet/Thermoforming Grade

Material Notes: INSPIRE 404 Performance Polymer is a propylene-based resin intended for use in thermoforming applications where exceptional stiffness, clarity and heat resistance is desired. The high stiffness of the resin may allow for the potential to down gauge and reduce part weight. The product is well suited for thin wall containers, serviceware and closure applications such as clear drink cups, deli containers, take-out containers, bowls and clear lids.

    Main Characteristics
  • Contains a nucleating agent
  • Excellent balance of stiffness and clarity
  • Superior heat resistance over conventional polypropylene
  • Complies with U.S. FDA 21 CFR 117.1520(c)3.2a (with Restrictions)
  • Canadian HPFB No Obligation

This product line was spun off from Dow Chemical to Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792
Melt Index of Compound 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 42.1 MPaASTM D638
Flexural Modulus, 1% Secant 2070 MPaASTM D790B
Izod Impact, Notched 37.4 J/mASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 129 °CUnannealed; ASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 16 %
@Thickness 1.00 mm
ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem INSPIRE™ 117 Performance Polypropylene Polymer
Dow INSPIRE™ 404 Performance Polymer
Braskem INSPIRE™ 114 Performance Polypropylene Polymer
Braskem INSPIRE™ 6025N Polypropylene Homopolymer
Braskem INSPIRE™ 6025 Polypropylene Homopolymer

PDOW0999 / 93334

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.