MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Danquinsa DANCURE® 246-12 Isocyanate Hardeners
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANCURE® 246-12 is a colorless isocyanate hardener for the cross linking of polyurethane-, polychloroprene- and natural rubber adhesives.

Application: DANCURE® 246-12 is distinguished by its long pot life in PUR- and polychloroprene adhesives. This property is especially useful in the two-component procession of adhesive primers which need up to 4 days to be heat-reactivated. As DANCURE® 246-12 is colorless and darkens only a little in case of light exposure, this cross linking agent is very suitable for light-colored materials.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.970 g/ccDIN 51.757
Solids Content 34 - 36 %DIN 53.189
Brookfield Viscosity 5.0 - 10 cPRVT
 
Thermal PropertiesOriginal ValueComments
Flash Point 1.00 °CDIN 51.755
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 4.01933
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
Aspectclear and colorless liquidity
Composition5.5-6.5%NCO
SolventEthyl acetate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ108 / 294528

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.