MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Halar® 9414 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE), Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; ECTFE Fluoropolymer

Material Notes: Halar® 9414 is a filled, pearl-white, semicrystalline melt processable fluorinated resin. It is designed for electrostatic powder coatings and can be used as a primer, intermediate or topcoat in protection and anti-corrosion applications.

Features: Good Chemical Resistance; Good Corrosion Resistance; Good Electrical Properties; Good Surface Finish; Good Thermal Stability; High Hardness; Semi Crystalline

Uses: Coating Applications

Additional Properties: Average Particle Size - Internal Method 28 µm

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.68 g/ccASTM D1505
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 275 °C
ASTM D1238
 
Thermal PropertiesOriginal ValueComments
Melting Point 242 °CDSC
 
Descriptive Properties
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 Latin America
 North America
ColorWhite
FormPowder
Processing TechniqueCoating

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Halar® 1450LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Syensqo (Solvay Specialty Polymers) Halar® 500 ECTFE Fluoropolymer
Vycom FLAMETEC™ HALAR® 901 Opaque Ethylene Chlorotrifluoroethylene (ECTFE)
Syensqo (Solvay Specialty Polymers) Halar® 930LCW Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Syensqo (Solvay Specialty Polymers) Halar® 3404DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE), Filled

PSOL8Y7104 / 176835

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.