MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPC 11812 S01 Polypropylene, Heterophasic Copolymer, Injection Molding
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Polypropylene PPC 11812 S01 has been developed for high speed injection molding of thin walled packaging containers requiring top level impact resistance at cold temperature (-20°C). It is characterized by a high Melt Flow index of 50 g/10 min, and allows an optimization of the injection parameters as for example a reduction of the cycle time, while keeping properties even at cold temperature (impact).

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.905 g/ccISO 1183
Bulk Density 0.525 g/ccISO 1183
Melt Flow 50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 24.0 MPaISO 527-2
Elongation at Yield 5.0 %ISO 527-2
Tensile Modulus 1150 MPaISO 527-2
Flexural Modulus 1100 MPaISO 178
Izod Impact, Notched (ISO) 6.50 kJ/m²
@Temperature -20.0 °C
ISO 180
 13.5 kJ/m²
@Temperature 23.0 °C
ISO 180
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C120°C per hour; ISO 752
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C120°C per hour; ISO 752
Vicat Softening Point 70.0 °C
@Load 5.10 kg
50°C per hour; ISO 306
 140 °C
@Load 1.02 kg
50°C per hour; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPR 9220 Random Copolymer Polypropylene, Injection Molding
Total PPC 10642 Polypropylene, Heterophasic Copolymer, Injection Molding
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade
Total PPC 5660 Propylene, Heterophasic Copolymer
Total PPC 11712 Polypropylene, Heterophasic Copolymer

PTOTAL858 / 130583

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.