SCG PP P443J is an impact copolymer polypropylene resin with good processing performance and excellent mechanical properties. It is particularly designed for injection molding and continuous compression molding of caps and closure for the packaging beverages. Applications: Caps and closures for carbonated soft drink and hot-filled beverages. Features: Good processibility. High stiffness. High heat resistance. With slip agent for good opening torque. Information provided by SCG. |