MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Eifeler Coatings Technology CrCN PVD Coating
Categories: Ceramic; Nitride; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Key Characteristics: low stress / good adhesion, high toughness and corrosion resistance

Primary Applications: drawing, pressing, bending and stamping of copper and other non-ferrous materials; metal forming of abrasive materials; plastic molding (improved mold release)

Information provided by Eifeler Coatings Technology

Key Words: chrome carbon-nitride
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 2.00 - 6.00 microns0.0787 - 0.236 mil
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 2100 - 25002100 - 2500
Coefficient of Friction 0.20 - 0.300.20 - 0.30dry, steel
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 600 °C1110 °F
 
Descriptive Properties
Colorsilver - gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tungsten Carbide, WC
Titanium Aluminum Nitride (TiAlN) PVD Coating

NEIFEL006 / 175961

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.