MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shandong Rike Chemical ACM-2 PVC Impact Modifier ACM Resin
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: For overcoming the shortcomings of plasticizers and CPE, this impact modifier ACM which as a copolymer of HDPE and acrylic acid was developed. ACM not only has the basic feature of CPE, but has higher impact strength and lower glass temperature compared to CPE, so its impact modification effect is more evident than CPE. Besides, ACM can effectively improve the weather-resistance of PVC products.

Application

The application method of ACM is the same as that of CPE. In processing, electric current and torque of extruders may have a slight decline and it may be eliminated through adjusting lubricant agent in the ingredients.

Information Provided by Shandong Rike Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Izod Impact, Unnotched (ISO) 17.9 kJ/m²
@Temperature 0.000 °C
Phr = 0
 19.8 kJ/m²
@Temperature 23.0 °C
Phr = 0
 20.6 kJ/m²
@Temperature 0.000 °C
Phr = 5
 22.6 kJ/m²
@Temperature 0.000 °C
Phr = 8
 24.6 kJ/m²
@Temperature 23.0 °C
Phr = 5
 25.8 kJ/m²
@Temperature 23.0 °C
Phr = 8
 
Descriptive Properties
Balance Torque (N-m)29.510 Phr
 29.78 Phr
 30.35 Phr
Fusion Temperature (°C)1778 Phr
 17810 Phr
 1795 Phr
Fusion Time (s)20210 Phr
 2118 Phr
 2355 Phr
Torque (N-m)25.1-31.68 Phr
 25.2-31.110 Phr
 25.3-32.45 Phr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Touchstone CFOAM® 17 Structural Carbon Foam
Saint-Gobain Rulon® ACM Bearing/Seal PTFE
Plastcom SLOVASTER® B/A GF 20 PBT, 20% glass fibre
Lanxess Rhenogran® KST-50/ACM (GE 1857) Rubber Processing Aid
Lanxess Rhenogran® Diuron-80/ACM Rubber Processing Aid

PSHAN076 / 103466

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.