MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 6011-75A Specialty Thermoplastic Elastomer, Wet-Grip Compound - Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: A Thermoplastic Elastomer specially formulated for Wet-Grip applications. Kinetic coefficient of friction against stainless steel when dry = 1.18 Kinetic coefficient of friction against stainless steel when wet = 1.04


Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/ccASTM D792
Linear Mold Shrinkage 0.0183 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 7510 sec; ASTM D2240
Tensile Strength at Break 1850 psi20 in/min (500 mm/min); ASTM D412
Elongation at Break 900 %20 in/min (500 mm/min); ASTM D412
Tear Strength 250 pliDie C; ASTM D624
Peel Strength 20.0 pliPolypropylene; Failure Type D; 90 degrees, 20 in/min (500 mm/min); ISO 813
Compression Set 15 %22 h 23 °C (73 °F); Method B Type 2; ASTM D395
 41 %22 h 70 °C (158 °F); Method B Type 2; ASTM D395
 
Processing PropertiesOriginal ValueComments
Melt Temperature 350 - 375 °F
Mold Temperature 70.0 - 100 °F
Drying Temperature 170 °F2 hrs
Injection Pressure 500 - 750 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Synprene® RT-3975 Thermoplastic Elastomer - SBC
API Megol AM DP1741 SEBS Adhesion Modified Overmolding for PA
Alliance Polymers Zythane™ 7075A Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 6075A Thermoplastic Polyurethane Elastomer
A. Schulman Alcryn® 2080 NC Melt Processable Rubber

PQZXA1768 / 58789

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.