MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Silfoam® SD 986 Silicone Antifoam Solution
Categories: Fluid

Material Notes: SILFOAM® SD 986 is a low viscous antifoam solution containing a low proportion of a highly viscous silicone fluid. The dimethylpolysiloxane contained in SILFOAM® SD 986 has a strong defoaming effect in numerous mineral oil products as well as in other non-aqueous systems, due to its low surface tension and good spreading ability.

Application: SILFOAM® SD 986 can be used in a variety of different applications, e. g. in applications in the oil field (crude oil / natural gas separators), in refinery processes (visbreaking, coking), in foaming distillation processes and in other foaming, non-aqueous formulations. Often, just a few ppm of SILFOAM® SD 986 will be sufficient for effective foam destruction.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.760 - 0.800 g/cc0.0275 - 0.0289 lb/in³
Solids Content 6.0 %
@Treatment Temp. 200 °C,
Time 900 sec
6.0 %
@Treatment Temp. 392 °F,
Time 0.250 hour
1g
Kinematic Viscosity 3.0 - 10 cSt3.0 - 10 cStDIN 51562
 
Thermal PropertiesMetricEnglishComments
Flash Point 62.0 °C144 °FISO 2719
Ignition Temperature 240 °C464 °Fliquids; DIN 51794
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.431.43DIN 51423
Transmission, Visible 90 %90 %"Clear" but manufacturer does not quantify.
 
Component Elements PropertiesMetricEnglishComments
Silicon, Si 2.3 %2.3 %
 
Descriptive Properties
Appearancecolorless, clear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9450 / 204979

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.