MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Superior Flux Ruby Fluid Paste Self-Cleaning Soldering Paste
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes: Description: Superior Ruby Fluid Paste is a Petrolatum-based soldering paste that contains Zinc Chloride. The Petrolatum helps protect the solder joint against corrosive attack and the paste form insures that the flux stays put until soldering.

Applications: Superior Ruby Fluid Paste is useful on most common metals except Aluminum and Magnesium. It is employed mainly in plumbing and maintenance applications. (Ruby Fluid Paste is available in pound cans, and in 5 lb., 20 lb. and 40 lb. pails.)

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 - 1.00 g/cc
 
Thermal PropertiesOriginal ValueComments
Boiling Point 337 °C
Flash Point 285 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 95.0 - 315 °CSoldering Range
Shelf Life 2.00 Month
 
Descriptive Properties
FormRed Paste
Spread Factor>80

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSFLUX125 / 185809

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.