MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polymer Resources TP-FR-IM Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Flame Retardant; Polybutylene Terephthalate (PBT), Impact Grade

Material Notes: Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Key Words: UL E113219
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/ccASTM D792
Linear Mold Shrinkage 0.010 - 0.014 cm/cmASTM D955
Melt Flow 3.0 - 9.0 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 6500 psiASTM D638
Tensile Strength, Yield 6500 psiASTM D638
Flexural Strength 11250 psiASTM D790
Flexural Modulus 290 ksiASTM D790
Izod Impact, Notched 10.0 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Gardner Impact 320 in-lbASTM D3029
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Strength 690 V/milASTM D149
Comparative Tracking Index >= 600 VUL 746
Hot Wire Ignition, HWI 7.0 - 15 sec
@Thickness 0.851 mm
UL 746
 15 - 30 sec
@Thickness 1.60 mm
UL 746
 30 - 60 sec
@Thickness 3.00 mm
UL 746
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 0.851 mm
UL 746
 >= 120 arcs
@Thickness 1.60 mm
UL 746
 >= 120 arcs
@Thickness 3.00 mm
UL 746
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/minUL 746
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 270 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 190 °FASTM D648
UL RTI, Electrical 266 °F
@Thickness 0.851 mm
UL 746
 266 °F
@Thickness 1.60 mm
UL 746
 266 °F
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 266 °F
@Thickness 0.851 mm
UL 746
 266 °F
@Thickness 1.60 mm
UL 746
 266 °F
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 185 °F
@Thickness 0.851 mm
UL 746
 185 °F
@Thickness 1.60 mm
UL 746
 230 °F
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-0
@Thickness 0.850 mm
 V-0
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 460 - 490 °F
Middle Barrel Temperature 470 - 500 °F
Front Barrel Temperature 480 - 510 °F
Melt Temperature 450 - 500 °F
Mold Temperature 110 - 180 °F
Drying Temperature 240 - 250 °F
Dry Time 3.00 - 4.00 hour
Vent Depth 0.000500 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow
LG Chemical Lupox® GP2300G PBT+GF30%
LG Chemical Lupox® GP2200 PBT+GF20%
LG Chemical Lupox® GP2100 PBT+GF10%
LG Chemical Lupox® GP1000A PBT

PPOLYQ249 / 160773

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.