MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Addolink® B PU Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Addolink B is used as a chain extender or crosslinking component for polyester and polyether casting elastomers (hot and cold) and for integral skin foam. The reaction between Addolink B and isocyanates leads to the formation of the hard polyurethane segments. The rapidity with which these hard segments are formed in the reaction mixture reduces the demolding time. The use of Addolink B also affects the physical properties of the finished product. It increases the material's hardness and improves the resistance to abrasion and heat. The addition of Addolink B depends on the needs of the finished product and can be varied between 2 and 10 parts by weight, calculated on 100 parts by weight polyol. As the freezing point of Addolink B is relatively high, temperatures above 22 °C are needed for satisfactory processing.

Function: Standard crosslinking agent for the production of polyurethane elastomers (hot- and cold-curing cast systems) and of integral skin foams.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/cc
Water Absorption <= 0.10 %
Viscosity 72 cP
 
Thermal PropertiesOriginal ValueComments
Melting Point 19.5 °CFreezing Point
Flash Point 135 °CASTM D93, DIN EN 22719
 
Descriptive Properties
Appearanceclear, colorless liquid
Hydroxyl value1245 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8209 / 208602

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.