MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Overview of materials for Polycarbonate, Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Carbon Fiber Reinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.21 - 1.75 g/cc0.0437 - 0.0632 lb/in³Average value: 1.30 g/cc Grade Count:129
Filler Content 5.00 - 50.0 %5.00 - 50.0 %Average value: 23.5 % Grade Count:21
Water Absorption 0.0500 - 0.300 %0.0500 - 0.300 %Average value: 0.110 % Grade Count:46
Moisture Absorption at Equilibrium 0.120 - 0.160 %0.120 - 0.160 %Average value: 0.145 % Grade Count:13
Additive Loading 15.0 - 30.0 %15.0 - 30.0 %Average value: 23.8 % Grade Count:8
Maximum Moisture Content 0.02000.0200Average value: 0.0200 Grade Count:4
Linear Mold Shrinkage -0.00100 - 0.00800 cm/cm-0.00100 - 0.00800 in/inAverage value: 0.00183 cm/cm Grade Count:102
Linear Mold Shrinkage, Transverse 0.000100 - 0.00800 cm/cm0.000100 - 0.00800 in/inAverage value: 0.00368 cm/cm Grade Count:52
Melt Flow 1.10 - 60.0 g/10 min1.10 - 60.0 g/10 minAverage value: 14.2 g/10 min Grade Count:13
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 100 - 125100 - 125Average value: 118 Grade Count:17
Tensile Strength, Ultimate 56.0 - 450 MPa8120 - 65300 psiAverage value: 139 MPa Grade Count:117
 65.0 - 115 MPa
@Temperature 60.0 - 120 °C
9430 - 16700 psi
@Temperature 140 - 248 °F
Average value: 92.5 MPa Grade Count:2
Tensile Strength, Yield 55.2 - 160 MPa8000 - 23200 psiAverage value: 115 MPa Grade Count:38
Elongation at Break 1.00 - 118 %1.00 - 118 %Average value: 4.06 % Grade Count:122
 1.30 - 1.70 %
@Temperature 60.0 - 120 °C
1.30 - 1.70 %
@Temperature 140 - 248 °F
Average value: 1.48 % Grade Count:2
Elongation at Yield 1.10 - 13.0 %1.10 - 13.0 %Average value: 3.45 % Grade Count:22
Modulus of Elasticity 2.14 - 48.0 GPa310 - 6960 ksiAverage value: 13.9 GPa Grade Count:95
 9.40 - 16.8 GPa
@Temperature 60.0 - 120 °C
1360 - 2440 ksi
@Temperature 140 - 248 °F
Average value: 13.0 GPa Grade Count:2
Flexural Yield Strength 51.7 - 660 MPa7500 - 95700 psiAverage value: 202 MPa Grade Count:127
Flexural Modulus 1.38 - 165 GPa200 - 23900 ksiAverage value: 12.9 GPa Grade Count:130
Compressive Yield Strength 131 - 215 MPa19000 - 31200 psiAverage value: 195 MPa Grade Count:5
Compressive Modulus 26.0 - 26.0 GPa3770 - 3770 ksiAverage value: 26.0 GPa Grade Count:3
Shear Strength 41.0 - 44.0 MPa5950 - 6380 psiAverage value: 43.3 MPa Grade Count:4
Izod Impact, Notched 0.320 - 2.67 J/cm0.599 - 5.00 ft-lb/inAverage value: 0.820 J/cm Grade Count:93
Izod Impact, Unnotched 2.67 - 16.0 J/cm5.00 - 30.0 ft-lb/inAverage value: 5.34 J/cm Grade Count:71
Izod Impact, Notched (ISO) 5.70 - 9.00 kJ/m²2.71 - 4.28 ft-lb/in²Average value: 6.82 kJ/m² Grade Count:11
 8.00 - 8.00 kJ/m²
@Temperature -30.0 - -30.0 °C
3.81 - 3.81 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 8.00 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) 29.8 - 39.9 kJ/m²14.2 - 19.0 ft-lb/in²Average value: 33.0 kJ/m² Grade Count:10
 30.0 - 30.0 kJ/m²
@Temperature -30.0 - -30.0 °C
14.3 - 14.3 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 30.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 1.00 - 5.00 J/cm²4.76 - 23.8 ft-lb/in²Average value: 3.37 J/cm² Grade Count:30
 4.50 - 4.50 J/cm²
@Temperature -40.0 - -40.0 °C
21.4 - 21.4 ft-lb/in²
@Temperature -40.0 - -40.0 °F
Average value: 4.50 J/cm² Grade Count:1
Charpy Impact, Notched 0.500 - 1.50 J/cm²2.38 - 7.14 ft-lb/in²Average value: 0.813 J/cm² Grade Count:31
 0.600 - 0.600 J/cm²
@Temperature -40.0 - -40.0 °C
2.86 - 2.86 ft-lb/in²
@Temperature -40.0 - -40.0 °F
Average value: 0.600 J/cm² Grade Count:1
Falling Dart Impact 2.26 - 31.2 J1.67 - 23.0 ft-lbAverage value: 14.2 J Grade Count:23
Instrumented Impact Total Energy 2.77 - 4.71 J2.04 - 3.47 ft-lbAverage value: 3.72 J Grade Count:7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0500 - 1.00e+12 ohm-cm0.0500 - 1.00e+12 ohm-cmAverage value: 8.34e+9 ohm-cm Grade Count:71
Surface Resistance 1.00 - 1.00e+12 ohm1.00 - 1.00e+12 ohmAverage value: 8.72e+9 ohm Grade Count:77
Static Decay 0.0100 - 2.00 sec0.0100 - 2.00 secAverage value: 0.824 sec Grade Count:19
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.00 - 72.0 µm/m-°C2.78 - 40.0 µin/in-°FAverage value: 19.8 µm/m-°C Grade Count:44
CTE, linear, Transverse to Flow 5.00 - 80.0 µm/m-°C2.78 - 44.4 µin/in-°FAverage value: 52.2 µm/m-°C Grade Count:29
Maximum Service Temperature, Air 120 - 150 °C248 - 302 °FAverage value: 127 °C Grade Count:19
Deflection Temperature at 0.46 MPa (66 psi) 101 - 152 °C214 - 306 °FAverage value: 144 °C Grade Count:71
Deflection Temperature at 1.8 MPa (264 psi) 86.7 - 149 °C188 - 300 °FAverage value: 138 °C Grade Count:101
Vicat Softening Point 111 - 155 °C232 - 311 °FAverage value: 146 °C Grade Count:23
Minimum Service Temperature, Air -40.0 °C-40.0 °FAverage value: -40.0 °C Grade Count:10
Glass Transition Temp, Tg 130 - 150 °C266 - 302 °FAverage value: 144 °C Grade Count:10
UL RTI, Electrical 80.0 °C176 °FAverage value: 80.0 °C Grade Count:20
UL RTI, Mechanical with Impact 80.0 °C176 °FAverage value: 80.0 °C Grade Count:20
UL RTI, Mechanical without Impact 80.0 °C176 °FAverage value: 80.0 °C Grade Count:20
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:76
 
Processing PropertiesMetricEnglishComments
Processing Temperature 249 - 310 °C480 - 590 °FAverage value: 283 °C Grade Count:13
Nozzle Temperature 254 - 327 °C489 - 620 °FAverage value: 293 °C Grade Count:19
Melt Temperature 135 - 332 °C275 - 630 °FAverage value: 295 °C Grade Count:70
Mold Temperature 35.0 - 130 °C95.0 - 266 °FAverage value: 92.2 °C Grade Count:78
Drying Temperature 70.0 - 130 °C158 - 266 °FAverage value: 117 °C Grade Count:73
Moisture Content 0.0200 %0.0200 %Average value: 0.0200 % Grade Count:51
Dew Point -28.9 °C-20.0 °FAverage value: -28.9 °C Grade Count:23
Injection Pressure 4.96 - 103 MPa720 - 15000 psiAverage value: 81.6 MPa Grade Count:33
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 inAverage value: 0.00514 cm Grade Count:14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, 10% Glass Filled
Overview of materials for Polycarbonate, Carbon + Glass Fiber Reinforced
Overview of materials for Polypropylene with 20% Talc Filler
Overview of materials for Polypropylene, Molded
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant

O3120 / 78137

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.