MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Monprene® CP-28964 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene CP-28164 is a clear high performance thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-28164 is a medium hardness grade that exhibits excellent sunlight resistance and UV absorbing characteristics, suitable for injection molding or extrusion.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Light Stabilized; Low Density; Low Specific Gravity; Lubricated; Medium Flow; Medium Hardness; Slip; Sunlight Resistant; UV Absorbing; Without Fillers

Uses: Consumer Applications; Gaskets; Handles; Kitchenware; Safety Equipment; Sporting Goods; Tubing; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ASTM D792
Melt Flow 14 g/10 min
@Load 5.00 kg,
Temperature 200 °C
14 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  67
@Time 5.00 sec
67
@Time 0.00139 hour
Injection Molded; ASTM D2240
 70
@Time 1.00 sec
70
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 5.10 MPa740 psi20 in/min, Flow; ASTM D412
 13.6 MPa1970 psi20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain  2.53 MPa
@Strain 100 %
367 psi
@Strain 100 %
20 in/min, Across Flow; ASTM D412
 3.52 MPa
@Strain 300 %
511 psi
@Strain 300 %
20 in/min, Across Flow; ASTM D412
 3.85 MPa
@Strain 100 %
559 psi
@Strain 100 %
20 in/min, Flow; ASTM D412
 4.76 MPa
@Strain 300 %
690 psi
@Strain 300 %
20 in/min, Flow; ASTM D412
Elongation at Break 390 %390 %20 in/min, Flow; ASTM D412
 780 %780 %20 in/min, Across Flow; ASTM D412
Tear Strength 34.5 kN/m197 pli20 in/min, Flow; ASTM D624
 39.4 kN/m225 pli20 in/min, Across Flow; ASTM D624
Compression Set  25 %
@Temperature 22.8 °C,
Time 79200 sec
25 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 46 %
@Temperature 70.0 °C,
Time 79200 sec
46 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Processing Temperature 199 - 249 °C390 - 480 °FMelt, Injection
Rear Barrel Temperature 182 - 232 °C360 - 450 °FInjection
Middle Barrel Temperature 188 - 238 °C370 - 460 °FInjection
Front Barrel Temperature 193 - 243 °C380 - 470 °FInjection
Nozzle Temperature 199 - 249 °C390 - 480 °FInjection
Zone 1 182 - 232 °C360 - 450 °FExtrusion
Zone 2 188 - 238 °C370 - 460 °FExtrusion
Zone 3 193 - 243 °C380 - 470 °FExtrusion
Zone 5 199 - 249 °C390 - 480 °FExtrusion
Die Temperature 199 - 249 °C390 - 480 °FExtrusion
Mold Temperature 35.0 - 48.9 °C95.0 - 120 °FInjection
Injection Pressure 1.38 - 5.52 MPa200 - 800 psiInjection
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceClear/Transparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0820 / 237311

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.